Flow accelerated corrosion rate on carbon steel pipe bend by thin layer activation technique and computational modeling: Under PHWR operating conditions

P. Madasamy,P. Chandramohan, M. Mukunthan,T.V.Krishna Mohan,S. Rangarajan, NirajUttam, R. Ramakrishnan, G. Babulal,H.P. Rani, P. Surendran, A.K. Gupta,J.P. Nair

Engineering Failure Analysis(2021)

引用 6|浏览4
暂无评分
摘要
•Carbon Steel pipe corrosion in 50NB Sch 160 of bend angle 58° radius 4 times diameter.•Specimen welded to HTHP loop irradiated with proton beam for nuclear reaction.•In loop pH (10.2) DO (<5 ppb) at 290 °C/87 bar maintained by adding LiOH and N2H4.•Corrosion rate measured by TLA method.•CFD simulated corrosion rate coincides with that of TLA method.
更多
查看译文
关键词
Carbon steel,Magnetite,PHWR,Thin layer activation,Flow accelerated corrosion