Depth-sensing ductile and brittle deformation in 3C-SiC under Berkovich nanoindentation
Materials & Design(2021)
摘要
The interplay between ductile and brittle deformation modes in hard brittle materials exhibits a strong size effect. In the present work, indentation depth-dependent deformation mechanisms of single-crystal 3C-SiC under Berkovich nanoindentation are elucidated by finite element simulations and corresponding experiments. A novel finite element framework, that combines a crystal plasticity constitutive model for describing dislocation slip-based ductile deformation and a cohesive zone model for capturing crack initiation and propagation-induced brittle fracture, is established. The utilized parameters in the crystal plasticity model of 3C-SiC are calibrated according to the load-displacement curves obtained from corresponding Berkovich nanoindentation experiments. Subsequent finite element simulations and experiments of nanoindentation jointly reveal co-existing microscopic plastic deformation and brittle fracture of 3C-SiC at different indentation depths, which significantly affect the observed macroscopic mechanical response and surface pile-up topography. In particular, the predicted morphology of surface cracks at an indentation depth of 500 nm agrees well with experimental observation, and the correlation of crack initiation and propagation with surface pile-up topography is theoretically analyzed.
更多查看译文
关键词
3C-SiC,Berkovich nanoindentation,Brittle fracture,Finite element simulation,Crystal plasticity,Cohesive zone model
AI 理解论文
溯源树
样例
![](https://originalfileserver.aminer.cn/sys/aminer/pubs/mrt_preview.jpeg)
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要