Atomic Layer Deposition Of Pbs Thin Films At Low Temperatures
CHEMISTRY OF MATERIALS(2020)
摘要
Atomic layer deposition (ALD) is a viable method for depositing functional, passivating, and encapsulating layers on top of halide perovskites. Studies in that area have only focused on metal oxides, despite a great number of materials that can be made with ALD. This work demonstrates that, in addition to oxides, other ALD processes can be compatible with the perovskites. We describe two new ALD processes for lead sulfide. These processes operate at low deposition temperatures (45-155 degrees C) that have been inaccessible to previous ALD PbS processes. Our processes rely on volatile and reactive lead precursors Pb(dbda) (dbda = rac-N-2,N-3-di-tertbutylbutane-2,3-diamide) and Pb(btsa)(2) (btsa = bis(trimethylsilyl)amide) as well as H2S. These precursors produce high quality PbS thin films that are uniform, crystalline, and pure. The films exhibit p- type conductivity and good mobilities of 10-70 cm(2) V-1 s(-1). Low deposition temperatures enable direct ALD of PbS onto a halide perovskite CH3NH3PbI3 (MAPI) without its decomposition. The stability of MAPI in ambient air is greatly improved by capping with ALD PbS. More generally, these new processes offer valuable alternatives for PbS-based devices, and we hope that this study will inspire more studies on ALD of non-oxides on halide perovskites.
更多查看译文
AI 理解论文
溯源树
样例
![](https://originalfileserver.aminer.cn/sys/aminer/pubs/mrt_preview.jpeg)
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要