Influence Of The Mechanical Properties Of Elastoplastic Materials On The Nanoindentation Loading Response
MATERIALS(2020)
摘要
The nanoindentation loading response of elastoplastic materials was simulated by the finite element method (FEM). The influence of the Young's modulus E, yield stress sigma(y), strain hardening exponent n and Poisson's ratio nu on the loading response was investigated. Based on an equivalent model, an equation with physical meaning was proposed to quantitatively describe the influence. The calculations agree well with the FEM simulations and experimental results in literature. Comparisons with the predictions using equations in the literature also show the reliability of the proposed equation. The investigations show that the loading curvature C increases with increasing E, sigma(y), n and nu. The increase rates of C with E, sigma(y), n and nu are different for their different influences on the flow stress after yielding. It is also found that the influence of one of the four mechanical parameters on C can be affected by the other mechanical parameters.
更多查看译文
关键词
nanoindentation,mechanical property,finite element method,elastoplastic
AI 理解论文
溯源树
样例
![](https://originalfileserver.aminer.cn/sys/aminer/pubs/mrt_preview.jpeg)
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要