Thermal cycling failure of three multilayer TBCs based on LaMgAl11O19 (LaMA)/YSZ was comparatively investigated by using the burner-rig testing method in this work. Results indicate that through optimizing the weight ratio and thickness of the intermediate LaMA/YSZ composite layers, a five-layer TBC with much improved thermal cycling life of 11,749 cycles at 1372 °C surface and 1042 °C bond coat testing temperature has been realized. While, thermal cycling lifetimes of the tri- and six-layer TBCs were 7439 and 7804 cycles at surface/bond coat testing temperatures of 1378 °C/1065 °C and 1367 °C/1056 °C, respectively. Factors related to the 60 wt.% LaMA + 40 wt.% YSZ (60LaMA + 40YSZ) intermediate composite layer with the highest thermal expansion coefficient than other composite layers generating higher internal stress level to the tri- and six-layer TBCs, different bond coat temperature and TGO growth, as well as long-term stability of the LaMA coating during thermal cycling tests, were characterized and compared to understand the different thermal cycling lifetime and failure modes among such three multilayer TBCs.
更多
查看译文
关键词
Thermal barrier coatings,Hexaluminate,YSZ,Thermal cycling,Plasma spraying
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要