Comparison between Ni-SALICIDE and Self-Aligned Lift-Off Used in Fabrication of Ohmic Contacts for SiC Power MOSFET

Materials Science Forum(2019)

Cited 1|Views58
No score
Abstract
A comparison between self-aligned process (using lift-off) and Ni-SALICIDE used in fabrication of ohmic contacts for SiC Power MOSFET is done. Both processes are demonstrated for 3.3 kV SiC VDMOS transistors fabricated on 100 mm substrates. It is shown that the Ni-SALICIDE process with first silicidation at 500 °C does not degrade the electrical properties of silicon dioxide; particularly, a degradation of the interlayer dielectric between source and gate is not evident. Additionally, this first silicidation is found to have a positive impact on the specific resistance of contacts formed on p-type SiC using NiAl2.6% as an ohmic metal.
More
Translated text
Key words
sic power mosfet,ohmic contacts,ni-salicide,self-aligned,lift-off
AI Read Science
Must-Reading Tree
Example
Generate MRT to find the research sequence of this paper
Chat Paper
Summary is being generated by the instructions you defined