西南某白云质胶磷矿高炉法还原工艺研究
Industrial Minerals & Processing(2013)
Abstract
对西南地区某白云质胶磷矿在高炉法磷酸工艺中的还原过程进行了研究,考察了还原反应温度、还原反应时间、硅钙比等工艺条件对还原效果的影响。结果表明,适宜的操作条件范围为:还原温度1400~1450℃,还原时间45~60min,硅钙比2~3。
MoreTranslated text
Key words
dolomitic collophane,reduction,blast furnace process