Abstract
The as-cast Mg-4Zn-2Gd-0.5Ca alloy mainly contained I phase and W phase, while the I phase dissolved into Mg substrate after homogenization treatment which improved the alloy's corrosion resistance. After the application of multidirectional forging (MDF), the grains were refined obviously accompanied with the precipitation of I phase. With the increasing pass of MDF, both the size of dynamic recrystallized grains and the amount of precipitated I phase increased. The corrosion resistance of Mg-4Zn-2Gd-0.5Ca alloy became worse after 1 pass of MDF as compared with the as-homogenizated condition because of the precipitation of I phase. Neverthless, the corrosion resistance of the as-MDFed Mg-4Zn-2Gd-0.5Ca alloy deteriorated with the increasing pass of MDF. As compared with grain refinement, the precipitated I phase is thought to play a main role on the corrosion behavior of Mg-4Zn-0.5Ca alloy. (C) 2018 Elsevier B.V. All rights reserved.
More
Translated text
Key words
Mg-4Zn-2Gd-05Ca alloy,Multidirectional forging,EIS,Corrosion resistance,Pitting corrosion
AI Read Science
Must-Reading Tree
Example
Generate MRT to find the research sequence of this paper
Chat Paper
Summary is being generated by the instructions you defined