Grain boundary properties of a nickel-based superalloy: Characterisation and modelling
Acta Materialia(2018)
摘要
Miniaturised tensile tests coupled with in-situ scanning electron microscopy are used to deduce the grain boundary properties of a nickel-based superalloy at 750 °C. This allows the damage initiation, evolution and failure processes to be observed directly. The significant variation in ductility – consistent with the limited number of grain boundaries being present – is rationalised using a crystal plasticity approach calibrated by experiments on single crystals loaded along the <001>, <011>, and <111> directions. Quantitative strength and toughness values for the grain boundaries are estimated using a cohesive zone method. The modelling approach is used to determine an approximation of the size of the representative volume element (RVE) needed for volume-averaged behaviour.
更多查看译文
关键词
Superalloys,Grain boundaries,Damage modelling,Crystal plasticity,Scanning electron microscopy
AI 理解论文
溯源树
样例
![](https://originalfileserver.aminer.cn/sys/aminer/pubs/mrt_preview.jpeg)
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要