The dry etching of GaN to form deep vertical structures is a critical step in many power device processes. To accomplish this, a chlorine and argon etch is investigated in detail to satisfy several criteria simultaneously such as surface roughness, crystal damage, and etch angle. Etch depths from 2 to 3.4 mu m are shown in this paper. The authors investigate the formation of etch pits and its contributing factors. In addition, a nickel hard mask process is presented, with an investigation into the causes of micromasking and a pre-etch to prevent it. The authors show the results of optimized etch conditions resulting in a 2 mu m deep, 0.831 nm rms roughness etch, with a 7.6 degrees angle from vertical and low surface damage as measured by photoluminescence. (C) 2016 American Vacuum Society.
更多
查看译文
关键词
gan,deep vertical etch,low damage,chlorine-based
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要