Low-temperature gas-barrier films by atomic layer deposition for encapsulating organic light-emitting diodes.
NANOTECHNOLOGY(2016)
Abstract
Dependences of gas-barrier performance on the deposition temperature of atomic-layer-deposited (ALD) Al2O3, HfO2, and ZnO films were studied to establish low-temperature ALD processes for encapsulating organic light-emitting diodes (OLEDs). By identifying and controlling the key factors, i.e. using H2O2 as an oxidant, laminating Al2O3 with HfO2 or ZnO layers into AHO or AZO nanolaminates, and extending purge steps, OLED-acceptable gas-barrier performance (water vapor transmission rates ∼ 10-6 g m-2 d-1) was achieved for the first time at a low deposition temperature of 50 °C in a thermal ALD mode. The compatibility of the low-temperature ALD process with OLEDs was confirmed by applying the process to encapsulate different types of OLED devices, which were degradation-free upon encapsulation and showed adequate lifetime during accelerated aging tests (pixel shrinkage <5% after 240 h at 60 °C/90% RH).
MoreTranslated text
Key words
atomic layer deposition,thin-film encapsulation,flexible electronics,organic light-emitting diodes,organic electronics
AI Read Science
Must-Reading Tree
Example
![](https://originalfileserver.aminer.cn/sys/aminer/pubs/mrt_preview.jpeg)
Generate MRT to find the research sequence of this paper
Chat Paper
Summary is being generated by the instructions you defined