Electrochemical properties of Atomic layer deposition processed CeO 2 as a protective layer for the molten carbonate fuel cell cathode
Electrochimica Acta(2014)
摘要
•Nano-structured CeO2-coated Ni by Atomic Layer Deposition, crystalline as-deposited.•Progressive transformation into a complex surface stable in molten carbonates.•Lower Ni solubility with CeO2 protective coating.•Feasibility of CeO2 coating in Molten Carbonate Fuel Cell cathode conditions.
更多查看译文
关键词
MCFC,Cathode,Cerium oxide,Coating,ALD,Electrochemistry