Influencing factors of coal gangue carbothermal reduction and nitridation reaction

Advanced Materials Research(2013)

引用 0|浏览3
暂无评分
摘要
Influencing factors of target products such as X phase, β′-SiAlON phase and O′-SiAlON phase of Inner Mongolia coal gangue carbothermal reduction and nitridation were researched by calculating the loss rate on ignition of specimens, and by means of XRD and SEM. During the carbothermal reduction and nitridation reaction of coal gangue, the loss rate on ignition of specimens rises with carbon reducer increasing, and keeping time has a little influence on the loss rate on ignition of specimens. If β′-SiAlON is target phase, the yield from corundum is much higher than that from special grade bauxite. Corundum or bauxite is used as starting material, the yield of X phase is low and the highest yield is only 12.88%. For the carbothermal reduction and nitridation reaction of coal gangue, the appropriate addition of reducer carbon is 10%-16%, and temperature influence is larger. The reaction temperature over 1420°C and keeping time of 6h are beneficial to the formation of X phase, β′-SiAlON and O′-SiAlON. © (2013) Trans Tech Publications, Switzerland.
更多
查看译文
关键词
β′-sialon,carbothermal reduction and nitridation method,coal gangue,influencing factor,o′- sialon,carbothermal reduction
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要