Q235等离子弧焊接工艺研究
Sci-tech Innovation and Productivity(2012)
Abstract
对6 mm厚的Q235碳钢,进行了等离子弧焊接试验,分析了Q235碳钢等离子弧焊接特点,并且对焊缝进行了X射线检验,研究了其力学性能及金相组织。
MoreTranslated text
Key words
keyhole effect,welding,plasma welding,Q235 carbon steel,welding procedure