云南某红土型风化钛砂矿选矿工艺研究

Nonferrous Metals(Mineral Processing Section)(2013)

Cited 0|Views23
No score
Abstract
在详细研究云南某红土型风化钛砂矿原矿性质的基础上,进行了多种试验室选矿工艺研究,弱磁—强磁—重选流程试验得到的钛精矿含TiO248.06%,回收率74.47%;弱磁—强磁抛尾后的粗精矿进行小型浮选闭路试验得到的钛精矿含TiO240.76%,回收率85.35%,选矿指标较好,为选厂的改造提供可靠的技术支持。
More
Translated text
Key words
pretreatment,weathered titanium ore,laterite ore,gravity concentration,de-sliming