基于数字图像处理的等离子喷涂NiCr-Cr3C2涂层纳米压痕有限元模拟
China Surface Engineering(2013)
Abstract
以等离子喷涂NiCr-Cr3C2涂层为研究对象,应用数字图像处理技术提取涂层孔隙分布形态,生成了包含孔隙在内的涂层有限元模型,并模拟计算了涂层纳米压痕压入过程.通过阈值迭代法、小波变换法和边界图形几何矢量化,提取了涂层真实细观结构的几何矢量图,并根据该结构图计算涂层孔隙率为6.88%.以提取的涂层矢量结构图为有限元模型基础,模拟纳米压痕试验加载过程,其载荷-位移曲线与试验曲线匹配性较好,表明该方法可将涂层微观结构和宏观力学性能结合起来.
MoreTranslated text
Key words
digital image processing,nanoindentation tests,plasma sprayed coating,simulation