优化旋流器结构参数提高磨矿细度的生产实践

Mining and Metallurgy(2007)

Cited 2|Views25
No score
Abstract
阿舍勒铜矿铜锌分离浮选作业入选细度要求高,需达到-0.043mm占95%。通过对磨矿生产流程的考察和计算,优化了再磨漩流器的结构参数,使再磨循环负荷提高了163.18%;旋流器溢流细度提高了2.87%,而且较好地解决了再磨机筒体、轴瓦发热的问题。
More
Translated text
Key words
structural parameters,grinding fineness,return sand ratio,Ashele copper mine,cyclones