铜尾矿蒸压砖的制备及影响因素探讨
Wall Materials Innovation & Energy Saving in Buildings(2006)
Abstract
以铜尾矿为主要原料,经过加压成型、蒸压养护制成承重标准砖,尾矿用量占固体原料总质量的85%,产品抗压强度16.1MPa,抗折强度3.8MPa,干燥收缩性能和冻融性合格。对影响产品性能的几个重要因素,包括成型压力、物料含水率和养护制度等进行了研究探讨。